News
Ore dressing test small shaking table|Locking the true value of the ore with just one "shake"
—— The "golden metronome" in the laboratory, making every gram of mineral sample speak up!
It's only half the size of a desk, but it can replicate the entire re-concentration process of the beneficiation plant.
6-S mini body, 0.4 m² bed surface, variable frequency 0-380 times/min, stepless adjustment of 0-25 slope;
0.02 mm fine sludge to 2 mm coarse sand, compatible with one bed;
Water consumption 0.3 t/h, noise 55 dB, can run quietly even in office buildings.
Water film ripple horizontal impact, triple layered mechanics, producing concentrate bands in 30 seconds, and stabilizing zoning in 5 minutes;
20-500 g feed per batch, recovery error within 1%, allowing you to pre-set factory indicators in the report.
304 stainless steel fiberglass bed surface, corrosion-resistant, wear-resistant, and non-clogging;
Quick-removable baffles, replaceable in 3 seconds with one hand, allowing you to switch from titanium-zirconium to rare earth immediately without cross-contamination;
Transparent PC cover, allowing full visibility of the process, and capturing it as a scientific research masterpiece with a single delay-shot on your phone.
USB direct connection to the computer, real-time recording of four parameters (stroke, frequency, slope, and water volume),
automatic generation of selectivity curves, and one-click export to Excel, eliminating the need for manual drawing of SCI illustrations.
Verified by 800 users from geological exploration, universities, mining companies, and recycled metal industries:
• In a lithium mica test, the original ore contained 0.92% Li₂O, and the small shaking table concentrate reached 4.8%, with a recovery rate of 78%, directly determining the factory specifications;
• In an African sand-tin project, the re-concentration indicators were obtained in 4 hours with a 30-kg sample, saving 20 tons of transportation costs for large machines;
• In the recovery of copper from electronic waste, the particle size was -0.5 mm, and the fine copper grade reached 92% with a recovery rate of 95%, passing the environmental impact assessment in one go.
Order now and get 3 sets of imported bed surfaces (coarse sand / fine sand / grooving), a portable inclinometer,
10 g gold standard samples, and hands-on teaching videos, with a 7-day no-questions-asked return and exchange policy.
The first step of mineral processing is to shake in the right direction.
The small shaking table for mineral processing — making mineral samples no longer "sink without a trace", and decisions no longer made "on the spur of the moment"!